Pd@ZnO core-shell structure, as synthesized Pd@ZnO is not fully crystalline, annealed at 500C-2h, Vacuum-Argon atmosphere, XRD patterns shows PdZn alloy peaks at 41 and 44 degrees. ZnO and Pd peaks are also present