At temperatures below 200 C oxidative degradation seems unlikely to play an important role. However, PLA is sensitive to humidity and can be hydrolyzed easily at the presence of water at high temperatures. If possible, your can try using antioxidants. The resin quality is also important. Monomers, oligomers and catalyst residues can catalyze the degradation reactions.