In DSC plots for chalcogenide glasses, the heat flow has positive value and increases with temperature. With heavy doping of foreign atom in chalcogenide glasses, the plots shows negative values of heat flow. What may be the reason for negative heat flow? Or what is the meaning of this type of changes?