I have been compressing SMA rod and it entered the strain hardening phase . i need to release this strain hardening , can this be done through the annealing process while maintaining its SME ?
Bala Narasimha Guniputi do you recommend a certain value below the austenite finish temperature to perform the annealing process ?
Another question to make sure i got you right ...if the annealing process is performed for a small interval of time ( 10 mins ) , it won't cause losing of SME ..did i got it right ?