The optimum conditions of depositions depend on the necessity of the properties of the thin film, the precursor you are using and the environment. At normal laboratory conditions the film properties can be controlled by spinning speed and number of deposition cycle. A spin rate around 1500 may yield highly transparent films with Cadmium acetate (BDH), 2-
It depends upon the precursor material you used, solvent, thickness of the film u needed.. the thickness of the film via spin coating depend upon number coatings, concentration of the solution, spin time, rpm value and so on....