FTO is more stable thatn ITO. but my concern is that the glass on which it is coated can withstand that temperature or not.
FTO can withstand 500 degrees Max. We use FTO procured from Sigma Aldrich and heat them in muffle furnace at 500degrees. The FTO withstand these high temperatures without a decrease of performance.
Dear Debarati roy chowdhury,
The melting point of FTO-coated glass is around 900 deg. C, which is mentioned in MATERIAL SAFTY DATA SHEET (MSDS), so please refer the attached file.
Instead of checking only the mRNA level, I want to check the active protein level of MMP-1 in Liver tissue from mice. How can I do that?
03 March 2021 1,763 2 View
I want to analyses the proportion of swimming sperm of three species of fish in two salinities. To analyse the proportion of swimming sperm in a Generalized Linear Model, I would use a Binary...
03 March 2021 2,297 3 View
03 March 2021 8,272 1 View
Hi. Please tell me what guidelines should i need to follow for questionaries' type research work in India. It is not hospital based work, we are conduction basic institutional based qualitative...
03 March 2021 2,037 3 View
Hi, I implemented a code to gabor filter cifar10 data but the images after being filtered and stacked are not clear like the original images. I think the problem is in the way I am using the...
03 March 2021 6,317 1 View
i am try to classify the x-ray images. During classification , can i block unwanted images (except x-ray image).
03 March 2021 7,100 1 View
03 March 2021 5,360 2 View
The term miscibility refers to the single-phase state in thermodynamics. I do not mean the compatibility of different components. To determine the miscibility I know several techniques such as...
03 March 2021 4,107 4 View
If the detection range is in ng/ml but the reference range is in ug/ml for a molecule or protein in serum or plasma .how to dilute and what is the initial volume to be taken for quantitative analysis
02 March 2021 7,670 3 View
02 March 2021 5,204 3 View
I want to do RF sputtering of ITO on glass substrate using magnetron sputtering. what thickness do i need to make it good conductive layer to use it for PSC. Moreover, whats about thickness of...
01 March 2021 395 3 View
Is the electropolymerisation of polyaniline coating over stainless steel (SS) via Cyclic voltammetry technique is really adherant? Else how to improve the adhesion of the coating, whether any...
01 March 2021 8,220 2 View
Increased heat, drought and insect outbreaks, all associated to climate change, have increased wildfires. Decreasing water supplies, declined agricultural yields, health impacts in cities owing to...
01 March 2021 7,168 9 View
Any idea on how to get the volumic ratio of glass fiber in a gypsum board ? Thank you for your help !
01 March 2021 2,501 3 View
Should I mesh the solid domain ? or should I use wall thickness? or Shell conduction? for Heat Transfer between two fluids of a Heat Exchanger. what is recommended?
01 March 2021 9,785 3 View
I want to cool Natural Gas from 195 Kelvin to 138 Klevin in a heat exchanger by using liquid nitrogen as the coolant medium. When entering the heat exchanger, the liquid nitrogen will have a...
01 March 2021 6,450 5 View
I am investigating thermospheric mass density profiles between 300-800 km altitude. I would like to compare the variability with other parameters, including temperature, electron content,...
01 March 2021 5,902 3 View
I have been trying to simulate heat transfer problem in Comsol 5.5 for long time but it always throw an error stating: "Failed to find a solution. Maximum number of Newton iterations...
28 February 2021 8,626 3 View
I am aiming to determine the ADC values of a commercial fish feed, but I do not have a steam pelleter or extruder available to me. Ideally, the pellets could be coated with some inert marker....
28 February 2021 7,967 3 View
Do we immerse the bricks horizontally or vertically ? #bricks#waterproofingsurface#civil#engeenering#chemicalengineering#wax#parafinwax
28 February 2021 6,685 2 View