Hi everyone, I have a question about a treatment that I am doing on aluminium parts, I have these aluminium (see image of the metalographic cut) pieces that I try to protect by anodization. After...
10 October 2018 4,572 3 View
I have deposited by CVD a graphene monolayer on copper ( I get a 2D/G of about 2,6) and after intercalation with an ammonium salt the ratio went up to 9.5. I would like to know your thoughts about...
03 March 2015 4,127 10 View
Is it normal to get fluorescence when I try to analyse my polymer grafted with pyrene by RAMAN? (We are getting a big fluorescence "contamination" when we try to analyse our polymer).