The SnO2 films that I have sprayed always have powder formation whenever at high temperature(>320℃) or low temperature(room temperature~150℃). The films are not smooth and like to be formed by...
14 July 2016 5,786 3 View
I prepare to fabricate SnO2 film by ultrasonic spraying a solution of SnCl2·2H2O in ethanol. But now uniform film can't be gained and many parameters such as temperature, flow rate etc. need to be...