Hi, I'm doing electrochemical reaction for the intercalation but i just found out that at some high voltages, solvent turns into black , especially for the solvent around the electrode. It looks...
12 December 2019 9,749 3 View
Hi. I'm doing an intercalation of Antiferromagnetic material using electrochemical reaction. But I just figured out after all experiment done, most crystals exfoliated on the substrate was gone....
11 November 2019 5,477 2 View
Hi. I did intercalation using NMP and crystal is attatched to the substrate using mechanical exfoliation. I did annealing after exfoliation so that crystal is attached to the substrate well. But...
10 October 2019 4,425 4 View