3 Questions 2 Answers 0 Followers
Questions related from Roksana Bavand
The source of the stress could be related to the further processing on top of the the thin film such as coating with resist, stripping the resist, baking, UV exposure, or oxygen plasma.
11 November 2018 1,795 4 View
I need to clean off my chips after coating two layers of photoresist and want to make sure that no more photoresist remains on the substrate. Is there any precise chemical analysis method to...
09 September 2017 1,220 4 View
Grey cast iron has a small amount of graphite that shouldn't be in nodular shape. By adding Magnesium (with less amount of Calcium) and Sulfur, the morphology changes to spherical. This morphology...