4 Questions 7 Answers 0 Followers
Questions related from Rishi Raj Raj
I have taken three pesticide imidacloprid, fipronil and chlorpyrifos stock solution in methanol and dilution buffer s Acetate buffer 0.5 M with 30% methanol and .2 M Kcl. I have applied negative...
07 October 2022 7,274 0 View
I have thermally deposited gold electrode on glass substrate with all the electrode ( RE, WE, CE) of same material i.e gold in microfludics devices. Now I want to check the cyclic voltammetry of...
16 May 2018 2,335 3 View
Not yet answered I have taken three pesticide imidacloprid, fipronil and chlorpyrifos stock solution in methanol and dilution buffer s Acetate buffer 0.5 M with 30% methanol and .2 M Kcl. I have...
01 January 1970 519 0 View
I was trying to deposit Cr and Au on glass substrate with thickness 30:70. I was getting some problem like:- 1. Au is not getting properly adhesion with Cr. 2. Tried with Ti and Au with...
01 January 1970 9,052 9 View