I have a powder which I guess to be a composite of an oxide ceramic with some polymers. I want their (the ceramic phase and the polymers) chemical composition and their weight percentage! And...
11 November 2014 3,783 9 View
Cast iron molds - being filled by large sand particles - are toughly degraded by erosion. Since the erosion is of brittle type toughness of the surface is of a great importance. Hardness is also...
09 September 2013 3,372 2 View
What are possible plating or any other surface engineering solutions to decrease surface degradation of cast iron molds through erosion by sand particles. As you may know, large sand particles...