6 Questions 2 Answers 0 Followers
Questions related from Raghad Al-Bayatti
I deposited CuS thin film using CBD technique . The precursor were 20ml of 0.1M CuSo4,20ml of 0.1M thiourea and 22ml of 25% ammonia.The resulted film after 1:30 minutes were non-uniform and...
07 July 2018 848 4 View
I need to download it.
10 October 2017 491 2 View
I deposited CdSe thin films using physical vapor deposition.I measured the transmission for as deposited films.Then I annealed deposited films under vacuum for one hour for different temperature.I...
10 October 2016 7,859 4 View
I deposited ZnS thin film on glass substrate using CBD and I calculated the thickness using weighing method as a pre calculation of thickness before using the accurate methods.I got an extreme...
10 October 2015 4,393 22 View
I deposited CdSe thin film using PVD technique and I measured the energy gap for the as-deposited thin films and after annealing for different temperature but constant time of annealing.The...
03 March 2015 3,484 5 View
I deposited the film using CBD ,but it's color does not change to yellow as expected.I changed the ratio of the chemicals but i got only white color not as supposed to be white to yellow color?
03 March 2015 8,691 4 View