I tried to filter the gold nanoparticle with cellulose acetate, 0.45 um filter. The hydrodynamic size of my nanoparticle are about 100nm (you can see the DLS analysis of them). The gold...
03 October 2019 7,373 7 View
As far as I know the PEG layer (or other functional group) can be formed in two ways on the surface of nanoparticles: mushroom or brush. Does this formation depend on whether the nanoparticle...
22 March 2019 6,111 3 View
To obtain tight packed DNA-gold nanoparticles, usually the salt-aging step is used. I would like to know if I can use the salt-aging step (or similar method) to increase the loading of thiol PEG...