4 Questions 10 Answers 0 Followers
Questions related from Onur Ozan Çilsal
I have been working on producing CNT's using a freshly designed cold walled CVD reactor. as catalyst I use iron nanoparticles. hot surface is graphite and temparature is between 500C and 700C. C...
09 March 2022 2,704 5 View
Attached I have some pictures of carbon nanotube that I produced with a coldwall CVD tank with ethanol vapour. Vacuum level was 250 pascals (not that low). Hot surface was a graphite plate around...
15 September 2021 2,365 8 View
I need a very hot surface to do CVD experiments for Carbon nanotube production Hot surface is in a vacuum tank I am using a AC Transformer which gives 1,5 Volt and 500Watts. Secondary coil is...
14 May 2021 6,945 11 View
I am planning to produce carbon nanotubes using the carbon inside the Ethanol. process is as follows: Inside the Vacuum Chamber, I will be placing 5ml liquid Ethanol. When I vacuum all the air...
17 April 2020 2,571 3 View