Which boundary in fcc has higher free energy: annealing or deformation twin? Any literature reference is highly appreciated.
02 February 2018 3,722 3 View
Steel grain boundary misorientation close to 60 degrees: is that necessarily a twin boundary? Can it be just a high-angle grain boundary?
01 January 2018 3,662 6 View
Which heat-treatment should be applied to 316L austenitic stainless steel in order to reduce or remove the defects after plastic deformation without recrystallization?
02 February 2017 5,659 6 View
Which heat treatment should be applied in order to increase the grain size in solution-annealed 316L steel?
11 November 2016 5,720 5 View
Which process leads to higher work-hardening rate of austenitic stainless steel: cross slip or planar slip?
08 August 2016 3,239 12 View
What is the reason of the occurrence of the banded structure in 316L austenitic stainless steel on the picture? Steel was hot-rolled and solution-annealed.
04 April 2016 323 11 View
I need to define the amount of ferrite in austenitic stainless steel. Which technique is better: EBSD or XRD?
11 November 2015 806 57 View
I am planning to measure the hardness of my steel samples. Do I need to do any specific surface preparation (grinding, polishing, etc.)?