3 Questions 5 Answers 0 Followers
Questions related from Nihal Khatiwoda
I was conducting PL analysis on the WSe2 monolayer and I see that the peak appears at 725nm in Fluoromax plus but when I use the Renishaw Invia Raman I see it at around 770nm. Please help.
13 August 2024 8,963 5 View
I wanted to know the best ways to locate the same CVD flake under an optical microscope in the material pre and post-experiments. It would be better if I could mark that flake without creating...
16 July 2024 9,191 2 View
I have a CVD-prepared material. The problem is that the LASER covers a smaller area than the islands, so I see localized effects. Sometimes, the intensity of the silicon peak is larger than the...
06 June 2024 6,855 3 View