Questions related from Muhammad Hilmi Johari
We have a Hitachi Arblade5000 broad ion beam milling system. I found that when we want to mill at the edges of a cross section, it will not mill properly. No matter how we do the sample alignment....
last month 1,331 1 View
I'm running a surface reaction. I'm wondering how does ANSYS Fluent calculate the surface deposition rate? Thank you.
14 July 2023 602 2 View
This is for CVD growth of MoS2 using the salt 2.0 technique. In literature, both of them have been used. But which is better for the growth of MoS2? Thanks.
02 November 2022 4,339 1 View
Most MSDS says that KBr is hygroscopic. Therefore, does it need to be stored in an inert (Ar, N) environment? Or storing it in a drybox is suffice? Appreciate your experience in storage and...
21 January 2022 8,468 3 View
I want to study the electronic, optical or catalytic properties of two-dimensional materials using MATLAB. What is the best way to start learning?
27 October 2020 1,983 8 View
I am currently doing a chemical vapour deposition of MoS2. The old tank with Argon gas has finished and has been replaced with a new one. All the growth using the new Argon gas are bad or none at...
30 January 2019 4,807 2 View