4 Questions 10 Answers 0 Followers
Questions related from Mohammad Zarei-Jelyani
How do you interpret a three-loop EIS for a graphite anode composite in Li-ion battery (after SEI layer formation)?
20 June 2019 8,380 0 View
I assembled a half cell of graphite anode. The charge/discharge cycles were performed in the voltage window of (2 - 0.01 V). The discharge capacity of coin-cell is more than its nominal capacity...
14 February 2018 4,648 5 View
I use a hot water bath to set temperature for charging / discharging a li-ion battery. but I'm looking for a way to surround the battery with air, not water. what is your idea for setting the...
26 July 2017 9,797 4 View
I assembled the coin cell in glove-box and my electrodes and seperator had not problem. I think the self-discharge is related to formation process of coin cell.
10 July 2017 3,668 6 View