2 Questions 1 Answers 0 Followers
Questions related from Mohammad Madiabu
Right after I attached ZnO in GPE surface, I tried the electrode to detect formaldehyde in aqueous solution with varied the supporting electrolyte (H2SO4 0.1 M, KCl 0.1 M, KOH 0.1 M, and some pH...
08 September 2024 4,858 0 View
I have been using paraffin, but the deposited ZnO still detach from electrode. What is the best binder to modify graphite paste electrode with ZnO nanoparticles?
04 August 2024 5,299 3 View