4 Questions 3 Answers 0 Followers
Questions related from Mohamed Shaaban
during Flash line cutting of forged valve super duplex stainless steel , there are certain procedure to follow to avoid creating internal defects inside valve, what are the related defects and...
29 April 2018 4,839 1 View
What possible damage mechanism rather than hydrogen em belittlement or HIC , if the secondary crack pass through ferrite of duplex only and principal crack is trans granular,
31 March 2018 3,621 2 View
hat is the failure mode and crack morphology of hydrogen induced crack in duplex stainless steel forged valve in hydrogen service ?
31 March 2018 9,458 2 View
What is the limitation of using PTFE with crystillized dinitrotoluene
13 November 2017 3,054 5 View