3 Questions 7 Answers 0 Followers
Questions related from Mandeep Singh
the pH of PBS is 7.4.
09 September 2014 7,564 0 View
I generally used zinc acetate dihydrate as a precursor for the ZnO thin film formation by spin coating technique . But it requires up to 450 C temperature for zinc oxide formation, otherwise at...
06 June 2014 7,268 9 View
I used zinc acetate dihydrate as a precursor.
10 October 2013 466 2 View