I am melting ferro alloys with mild steel to form a specific composition But the final product has high sulphur content leading to detrimental inclusions. Is any way or industrial practice to...
04 October 2016 1,163 7 View
I have a sample of size 32 x 32 x 24mm. Ideally for austenitization , the holding time is decided based on sample size but is there a thumb rule ? And for transformation at a given temperature,...
01 June 2016 6,587 17 View
For any diffraction pattern, using "search and match" in software shows the possible phases (based on restriction). But when we accept a phase We can see the score and scale value. What does it...
06 May 2016 9,264 7 View
Suppose I get a structure with Martensite and Bainite. I tempered it . Now how can i differentiate between the tempered martensite and bainite as both looks same however the mechanism of formation...