We usually use the Cu foil (80um) for growth of h-BN by using horizontal flow - CVD. There is a problem. It is that the Cu deposited on the quartz during the CVD process. To remove the Cu as...
08 August 2019 7,900 5 View
We usually grow h-BN on Cu foil using CVD system. I don't know what is the problem. Typically, Our Cu foil is poly-crystalline with 100um thickness. When we take sample out in the quartz tube of...