I'm willing to use XRR measurements as alternative method to measure thickness of a thin film. But still I couldn't get a good fringes pattern. Since one of the major factor affecting to the...
08 August 2019 4,420 23 View
Can anyone advice me about the JCPDS - ICDD PDF number of Fluorine doped Tin Oxide (FTO) so that I can find the standard XRD pattern from the inbuilt software of the XRD machine. I couldn't find...
06 June 2019 5,056 4 View
Could you please suggest me whether will it suitable to perform after deposition treatment for CdS deposited layer before consider next layer (probably CdTe) and if so, what are the possible after...
01 January 2019 5,457 7 View
In my research which based on polymer electrolytes, I have do dissolve Magnesium trifluoromethanesulfonate (MgTF) in a methyl-grafted natural rubber (MG49) which already dissolved in Toluene. But...