3 Questions 1 Answers 0 Followers
Questions related from Hussam Alnammary
PTFE is exposed to hot concentrated sulfuric acid and was found blistering . Based on my undestanding, plastic materials are permeable and can contain microvoids, which are the possible main...
05 September 2019 4,435 3 View
U-PVC pipe is used for chlorinated HCL 14% at 55 c, and blisters are formed on the internal surface of the pipe after a year of service. What kind of reaction that may occur that could explain...
22 May 2018 9,936 0 View
Multiple webpages (Including Wiki) state that FEP & PTFE do not withstand repetitive folding. Is the statement correct? and what would be the effect on the materials characteristics?