When I am trying to make PVDF film, after heating it seems to cracked and the white thick cast occured instead of glassy thin film. I am using 1gm pvdf with 8 ml DMF and 2 ml Acetone. And the...
19 May 2023 8,280 1 View
Initial solution was prepared by dissolving 5 mmol of Sr(NO3)2 and 10 mmol of Fe(NO3)3·9H2O in 15 mL deionized water and the mixture was subjected to vigorous magnetic stirring to obtain a clear...
27 March 2023 8,529 0 View
How to analyse this combine TG-DSC curve. I can find only one weight loss step? how to interpret this graph. This is done for my ferrite sample calcinated at 600 degrees celsius.
20 November 2021 297 3 View
When I go through the XRD data match using Xpert highscore plus I got a file match of 49 scores for my undoped ferrite sample. Is it valid to my prepared sample. ? Also how could I find the effect...