I rolled the Cu foil to different thickness reductions. XRD peaks were shifted to lower angle with the increase in thickness reduction. What Can be the reason?
08 August 2018 9,106 3 View
HOW TO PRODUCE Ni(OH)2 nanostructures on Ni foil . People are dipping Ni in LiOH solution to get Ni(OH)2, but we are not getting green colour
08 August 2016 1,967 0 View
I have Cu and Ni shots (balls), I want to remove oxide layers from them. Please tell me the solution
04 April 2016 3,448 2 View
Please tell me the name or author of good physics books. I like to make to collection of all good physics book so that one can teach what physics actually is Please suggest me books on Condensed...
09 September 2015 4,935 3 View
Labosoft is a software for texture analysis, I am not getting it Please tell me how to get it. Thanks
09 September 2015 9,353 0 View
For making alloy of Cu,Co and Ni through vaccum arc melting, i am using shots of about 1.2 cm size, so before melting what type of cleaning is required before meting for cu shots, Co shots and Ni...
08 August 2015 3,031 4 View