I used one step spin coating deposition method with Chlorobenzene anti-solvent to fabricate MAPbI3 perovskite...However, after deposition, these waves were formed in my layers ... can anybody says...
25 September 2016 7,720 10 View
high conversion efficiency in my idea is sth more than 14%
01 June 2016 5,802 4 View
I know the diffusion length of perovskite layer is about 1 micrometers. And I know the thickness range for this layer is about 300 nm to 1 micron. However I am curious to know if it's possible to...
20 December 2015 813 3 View
Simulation, DSSCs