Silicon substrate was cleaned prior to deposition to remove native oxide. Off-axis (90 degree) PLD was performed at around 50 m.Torr oxygen partial pressure, 1 J/S.cm fluences and 500 C...
17 December 2013 1,005 6 View
People demonstrated epitaxial BST/Si using MBE but not with PLD.