1 Questions 7 Answers 0 Followers
Questions related from Donald Robinson
Major problem is delamination in 0.1 M HNO3 (pH 1). Added kudos for more cost-effective approach. desired Pt film thickness: 100 nm desired stability: pH range (1-13), solvents (water, neutral...
08 August 2015 1,848 5 View