3 Questions 6 Answers 0 Followers
Questions related from Dhineshkumar Ramesh
I made FG coating with LTA and YSZ. I would like to observe OM and SEM images. Polishing does not reveal the FG layer so Etching is necessary. So please tell me the etchant details. Thank you in...
11 November 2014 2,747 1 View
1) La2o3 heated 1100C for 5h previously and three powders are ball milled for 3h and dried for 70c 2) Three powders mixed at 1650C for 24h and ball milled with arabic gum and deionized water and...
05 May 2014 7,030 1 View
For TBC coating with combination of YSZ and LaMa as top.
04 April 2014 8,938 3 View