3 Questions 1 Answers 0 Followers
Questions related from Dheeraj Kumar
I did annealing of polyethylene of 200um(size 2x2 mm) on Silicon at 300 °C for 10 min. After the annealing process i saw the thickness of polyethylene increased to 500um approx!!!!!! Can anyone...
11 November 2017 429 3 View
I need to clean HDPE film so to remove the absorbed gases and other contaminants from the surface of HDPE film without changing its physical and chemical property.
03 March 2017 7,380 0 View
Whether radiation destroy silicon-glass bonding? Is there any chemical reaction going which create defect on the bonded silicon-glass surface?
01 January 2017 2,272 1 View