We deposited ZnO on Si, and observed a thikening of interface SiOx when annealing morethan 500℃. I'd like to analize why this temperature is specific, I don't know how to describle it.
02 March 2024 6,352 2 View
When we chose materials to form contact with silicon,sucn as metal, TCO or some other semiconductors, which parameter is choiced for the band alignment. So far I know that when metal comes into...