3 Questions 1 Answers 0 Followers
Questions related from Atakan Barkınay
Hello. I continue a long time to sol-gel superhydrophobic coating. In the lab, has not the dip coating and spin coating machine. That's why I using a tweezer but my samples aren't straight. How...
01 April 2022 7,528 0 View
Hi I working on Titanium sol gel. I dried glass at 100 Celcius for an hour and calsination at 500 Celcius for an hour. After this process, the glass is waiting in furnace all day for cooling. When...
20 January 2022 6,831 1 View
I'm working on superhydropobic coating with titanium sol-gel. I use titanium isopropoxide, ethanol, distilled water and HCI. After dip coating, I put glass to in desiccator and dried 50 C for 1...
08 November 2021 7,407 2 View