5 Questions 24 Answers 0 Followers
Questions related from Ashish Gupta
What is possible if no plateau observed in ist discharge cycle carbon as anode in lithium ion half cell. however irreversible capacity loss occurs
07 July 2017 2,857 3 View
is immediately after cell fabrication the li ion goes to the carbon? and so when we carried out first cycle it is discharging (lithium goes back to anode). or in discharging lithium ions got...
06 June 2017 6,112 9 View
At higher temperature heating in inert, 42 peak get suppressed while 44 peak arises. is 42 peak related to defects in the carbon crystallography?
07 July 2016 3,596 9 View
Nanofibers diameters are in the micron range i.e. 200-1000nm and their length is in meters or centimeters. Why are they called nanofibers when the nano prefix added to them has a size of up to 100nm?
01 January 2013 9,166 2 View
when it is perfect layers are straight but if layers are scrumbled. is this a kind of defect. if yes, then what kind of defects can be observed? any reference...