why peak area is considered instead of peak intensity in FTIR for calculation of electroactive phase of PVDF? Is it possible to calculate percentage of beta phase using XRD pattern.
19 March 2025 6,306 1 View
I am working on using raw keratin powder as a filler in film composites. However, keratin is not soluble in DMF, likely due to the presence of disulfide bonds. I need to cleave these disulfide...
31 January 2025 2,138 0 View
I am working with PVDF films, which I prepare using DMF at 65°C. sometime, in the FTIR analysis of these films, a flat curve appears in the region where the beta phase peak is expected. What could...
24 September 2024 9,442 2 View
I am working on polymer, i want to make film of PVDF so i made solution at 65 degree but it turns into gel when left for sometime at room temperature in open atmosphere. i am using DMF as solvent....