I prepared a film with PEDOT:PSS after adding EG into it (3%). I noticed that the ac conductivity measured for the film sample of thickness in the range of 50 microns is very less and in the order of 10^-9. I prepared the film after filtration using PVDF syringe filter as the dispersion was not giving a uniform film. Could that be the reason for reduced conductivity?