2A02 aluminum alloy was water quenched at 500℃ and then aged at 170℃ for 16 h. No precipitated phase was found under TEM.I wonder what is the reason for this. Help me,please
06 April 2021 7,657 3 View
After the dissolution and aging of the precipitated phase, I would like to ask you what phase this is?