Now I am facing with the limitation of cooling length zone for fast firing kiln and need to figure out which zone of cooling causes more severe cooling crack. Quartz inversion at 573 degree C...
24 March 2016 4,220 2 View
I have a controversial studies between peak position and lattice strain in Li-doped ZnO. the XRD peak of Li-doped ZnO in lower meaning that it's in tension resulting from interstitial defect...
05 October 2014 7,808 6 View
I have found that Ga-doped ZnO can cause tension in lattic both high and low doping concentration as Li+ does. Some literature talks about formation energy. Some discuss the size and...