2 Questions 6 Answers 0 Followers
Questions related from Swayamprava Dalai
I am trying the sol-gel process using TTIP as the precursor, with Ethanol and HCl. however, the annealing furnace is out of order. Can anybody suggest some alternate method?
11 October 2018 2,335 16 View
I have prepared PLGA-PVA nanoparticles of size 140-180 nm. PLGA nanoparticles were prepared by centrifuging at 28000 rpm at 4 degree C for 30 min, using double emulsion method. I am facing problem...
01 January 1970 7,098 2 View