2 Questions 3 Answers 0 Followers
Questions related from Sukhvinder Singh
I have deposited double layer, first Fe and then Ni (both around 100 nm thick) on Si substrate. Then I will do heat treatments to expect formation of alloy of Ni and Fe (i.e., Permalloy). Which...
10 March 2021 5,647 5 View
I am using Nanoscope 4 Multimode AFM. The laser clearly reaches (after reflection from cantilever) the photodiode, but SUM signal is always zero. Also Vertical and Horizontal signals do not...