I've been using the same 1" tube furnace to carbonize my polymer nanofibers. I follow a typical protocol where I first stabilize the sample in a box furnace (in air) at 280 C then use the tube...
09 January 2019 2,992 4 View
I'm using the commercial GOx activity assay from Sigma Aldrich. I'm testing both commercial GOx just dissolved in PBS and GOx immobilized on my electrode nanomaterials. The absorbance at 570nm...