Hi , I want to characterize the cross-section of the Cu foil by SEM to determine the thickness of the oxide layer. I don't know how to cut the foil without damage the cross-section. I used scissor...
05 September 2018 9,314 8 View
I performed a DSC analysis of PCM(nitrate salt). In the results of the previous paper, the crystallization temperature of this material is 240 ℃. but my result was about 180℃. what's the...