3 Questions 10 Answers 0 Followers
Questions related from Somashekara koushik Ayalasomayajula
I performed FE-SEM on hollow fibers and observed that some areas are not sputtered. Au/Pd alloy was used for sputtering. What could be the possible reason for such a scenario. Regards, Koushik...
09 October 2016 5,387 11 View
In order to comment on surface hydrophilicity of PSf/PVP based hollow fiber membranes (porous) for Ultrafiltration, what could be the best method to evaluate contact angle.
09 August 2016 5,771 4 View
Hollow fiber membranes produced by dry wet spinning technique PSf as base material, PVP as additive and DMAc as solvent, show a reduction of performance once they are stored for 2-3 weeks after...