2 Questions 3 Answers 0 Followers
Questions related from Shalin P Marathe
I have Friction stir welded blanks from AA 6061 T6. The blank thicknesses are 0.5, 1 and 1.6 mm. After welding, it has been observed that the joints are very brittle. I want to improve the...
25 July 2019 3,009 3 View
I am trying element deletion in ABAQUS using ductile damage criteria. Can any one help me to understand the meaning of the term "displacement at failure" considering ABAQUS terminology ? For...
17 October 2017 8,459 16 View