1 Questions 3 Answers 0 Followers
Questions related from Sandhya Adhikari
I have successfully coated the Fe304@Sio2@PPy( Polypyrrole) simply by taking 100mg Fe304@Sio2 ,suspended in 15 ml DI water then sonicate for 15 min then add 100 microlitre pyrrole. Solution was...
01 January 2020 2,373 6 View