Hello, I have some SAED patterns taken from ZrN/Cu coatings deposited by reactive magnetron sputtering. When there is a preferred orientation in the microstructure, the corresponding ring is not...
03 May 2022 267 3 View
Hello, I have deposited some ZrN coatings with different amounts of Cu (0-30 at.%) by reactive magnetron sputtering. In the XRD patterns, I can see the shift to the higher diffraction 2-thetas but...
25 March 2022 6,771 9 View
I am working on some bactericide coatings which contain various amounts of copper. The goal is to observe the bacteria-killing efficiency of the coatings with copper content and exposure time for...