6 Questions 9 Answers 0 Followers
Questions related from Saad Saadsaad
I wanted to make triethanolamine oleate as a lubricant. So I purchased oleic acid. There were two different oleic acid (industrial grade) in the maket: liquid and semi-solid. What is their...
09 September 2018 7,467 0 View
Hi to all Sometimes a few bubbles create in the glassy articles produced through melting method. The glass refining conditions are usually required to remove it. Sometimes, however, the bubble is...
02 February 2018 1,590 8 View
Hello to all I am investigating about metallic rod coating with glass. The thermal expansion of metal and glass are equal approximately. What's your idea about a tight and sticky coating? Thanks...
08 August 2017 7,268 8 View
Hello to allI seek for furnace maker specially for AZS brick (zac refractory).For producing AZS refractories an electrical arc furnace (EAF) is necessary. I need a EAF for 5-10 tonne/day AZS...
07 July 2017 6,970 4 View
Hi, I want to perform a process in that molten glass flows on ceramic vessel. Here after 1 week the ceramic vessel is corroded and deteriorated. What is a good thermal barrier against molten...
05 May 2016 8,102 9 View
I want to study YSZ crystal with MD in Materials Studio, but I don't know how to build YSZ first crystal.
11 November 2013 8,223 3 View