I have coated SUH 3 and SS-AISI-321 metals with a 50-micron NiCr layer followed by a 100-micron layer of YSZ, a 50-micron NiCr layer followed by a 100-micron layer of Lanthanum Zirconate, and a...
22 August 2023 2,513 1 View
I'm preparing lanthanum zirconate in 1:2 mole ratio of La, Zr in a tungstan carbide vial using ball milling method. Initial one hour of run showed that the powder was sticking to the Vial and...